Posts: 17786
Topic starter  


   
john barry
(@john-barry)
Illustrious Member
Joined: 6 years ago
Posts: 12783
 

Have you considered felt ?



   
(@phil-r)
Illustrious Member
Joined: 6 years ago
Posts: 17786
Topic starter  


   
Rick Scoville
(@topgun1954)
Famed Member
Joined: 30 years ago
Posts: 2596
 

Phil, usually (especially for the application you're looking at), the flocking process is multi-step. The surface would be stripped clean. You'd then apply either a solvent-based or water-based adhesive to the plastic (ABS/surlyn/PVC, etc) glove box. At that point, the flock would be electrostatically applied and then cured for bonding.

Never have heard of a flocking-in-a-can product. Whatever you use, it would have to have some type of electrical charge in order to make those flock fibers stand up to give you that "felt" feeling/surface.

Hope you find something that works.



   
(@phil-r)
Illustrious Member
Joined: 6 years ago
Posts: 17786
Topic starter  


   
(@Dave VanderWal)
Joined: 1 second ago
Posts: 0

   
Rick Scoville
(@topgun1954)
Famed Member
Joined: 30 years ago
Posts: 2596
 

Phil, I sold flock adhesives into the automotive industry for 35 years. I can say with utmost certainty that the process I described is how Ford suppliers (or GM, Daimler/Chrysler/Honda/Toyota/BMW, etc) flocked consoles, door panels, glove boxes, etc. Depending on the substrate (ABS, suryln, PCABS, etc.), the primer varied, but the actual flocking process was the same across the board. Same for the window weatherstrip on your car or truck. The extrusion is primed or buffed and then a flock adhesive is applied, flocked then cured. Some suppliers have moved to co-extruded felt strips bonded directly to the extrusion (usually EPDM or synthetic polymer).

That said, I'm not sure how Franklin Mint or Danbury obtained that "flocked" feel. Perhaps someone like George B. could enlighten us.



   